Thermal Expansion Behaviour of Ce2Zr2O7 up too 898 K in Conjunction with Structural Analyses by Neutron Diffraction

cover
The thermal expansion of cubic pyrochlore Ce2Zr2O7 has been measured from room temperature to 898 K on polycrystalline material in conjunction with structural analyses using neutron diffraction. This compound has a thermal expansion coefficient in line with the other comparable lanthanoide pyrochlore oxides. The coefficient can be expressed as ¿(T) = 8.418×10-6 + 0.9861×10-9×T. The structural refinements performed for each measured temperature showed a comparable linear evolution of the Ce-O / Zr-O distances (within 0.57%).
2010-11-09
SPRINGER
JRC54503
0342-1791,   
https://publications.jrc.ec.europa.eu/repository/handle/JRC54503,   
10.1007/s00269-010-0356-5,   
Language Citation
NameCountryCityType
Datasets
IDTitlePublic URL
Dataset collections
IDAcronymTitlePublic URL
Scripts / source codes
DescriptionPublic URL
Additional supporting files
File nameDescriptionFile type 
Show metadata record  Copy citation url to clipboard  Download BibTeX
Items published in the JRC Publications Repository are protected by copyright, with all rights reserved, unless otherwise indicated. Additional information: https://ec.europa.eu/info/legal-notice_en#copyright-notice